Polyethylene films are one of the most frequently used packaging materials in our society, due to their combination of strength and flexibility. An unintended consequence of this high use has been the ever-increasing accumulation of polyethylene films in the natural environment. Previous attempts to understand their deterioration have either focused on their durability using polymer analysis; or they have focused on changes occurring during outdoor exposure. Herein, this study combines those strategies into one, by studying the chemical and physical changes in the polyethylene structure in a laboratory using molecular weight and IR spectroscopic mapping analysis, combined with temperate UV-accelerated weathering cycles. This approach has been correlated to real-world outdoor exposure timeframes by parallel testing of the sample polyethylene films in Florida and France. The formation of polyethylene microparticles or polyethylene waxes is elucidated through comparison of drop point testing and molecular weight analysis.

Iaith wreiddiolSaesneg
Rhif yr erthygl2373
CyfnodolynPolymers
Cyfrol13
Rhif cyhoeddi14
Dynodwyr Gwrthrych Digidol (DOIs)
StatwsCyhoeddwyd - 20 Gorff 2021
Cyhoeddwyd yn allanolIe

Dyfynnu hyn